| Parameter | Value |
|---|---|
| Orderable part number | HC7-1R0-R |
| OCL (open circuit inductance) | 1.05 uH ±20% |
| Irms (DC, 40 °C rise) | 20.3 A |
| Isat (15% rolloff) | 19.6 A |
| Isat2 (30% rolloff) | 37.1 A |
| DCR typical @ +20 °C | 2.1 mOhm |
| Volt-time rating (V-us) | 5.36 |
| Package | 13.8 mm long |
| Height | 5.5 mm |
| Mounting | Surface mount |
| Operating temperature | -40 °C to +155 °C (ambient plus self-heating) |
| Qualification | Commercial grade |
| RoHS | Compliant, -R suffix |
| Data sheet | Eaton Technical Data 4116 |

Drawing reproduced from Eaton Technical Data 4116: outline with
rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
the drawing itself.
A powder core with a non-organic binder is a deliberately conservative choice: it trades a little permeability for predictable behaviour at high current and high temperature. The result is an inductor that stays linear enough for a current-mode loop to be designed around it.
Copper loss at the rated current works out to roughly 0.865 W from a typical DCR of 2.1 mOhm at 20.3 A. It is the number to start a thermal stack-up with, before core loss and before AC resistance rise.
Isat is specified as 15% rolloff, so the number is a rolloff criterion rather than an absolute maximum. The useful working range extends a little beyond it on a soft saturation core, but the loop compensation has to be designed for the inductance that remains.
Energy storage at the saturation current is around 202 uJ, the number that connects the inductance and the current rating into a single transient figure.
The second saturation column, 37.1 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.
The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.
The HC7 family spans 0.22 uH to 4.81 uH; this row sits at position 3 of 7.
The next value up in the same family, HC7-1R5-R, gives 1.73 uH at 14.2 A and DCR 4.3 mOhm: the extra inductance costs about 9.2 A of rated current.
Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 2.1 mOhm becomes roughly 3.21 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.
Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.
How do I estimate the inductance at my operating current?
Read it off the inductance-versus-DC-bias curve in the data sheet at the actual bias. The curve, not the OCL value, is what sets the ripple at load.
Does the inductance drift with age?
The binder is non-organic and the core is not gapped with adhesive, so thermal aging of the magnetic path is not a mechanism here. The value is stable across thermal cycles.
Why is the DCR higher than a ferrite part of the same size?
Iron powder has lower permeability, so more turns are needed for the same inductance, and more turns mean more copper. The compensation is the much higher saturation flux density.
Shenzhen Gaorunxin Technology Co., Ltd
Shenzhen Gaorunxin Technology Co., Ltd