| Parameter | Value |
|---|---|
| Orderable part number | HC7-R20-R |
| OCL (open circuit inductance) | 0.22 uH ±20% |
| Irms (DC, 40 °C rise) | 35.8 A |
| Isat (15% rolloff) | 45.8 A |
| Isat2 (30% rolloff) | 86.5 A |
| DCR typical @ +20 °C | 0.67 mOhm |
| Volt-time rating (V-us) | 2.27 |
| Package | 13.8 mm long |
| Height | 5.5 mm |
| Mounting | Surface mount |
| Operating temperature | -40 °C to +155 °C (ambient plus self-heating) |
| Qualification | Commercial grade |
| RoHS | Compliant, -R suffix |
| Data sheet | Eaton Technical Data 4116 |

Drawing reproduced from Eaton Technical Data 4116: outline with
rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
the drawing itself.
Powder iron is the material choice that gives this family its soft saturation curve and its stable inductance over temperature. There is no thermal aging of the binder, so the inductance you measure on day one is the inductance you have after a thousand thermal cycles.
Copper loss at the rated current works out to roughly 0.859 W from a typical DCR of 0.67 mOhm at 35.8 A. It is the number to start a thermal stack-up with, before core loss and before AC resistance rise.
Isat is specified as 15% rolloff, so the number is a rolloff criterion rather than an absolute maximum. The useful working range extends a little beyond it on a soft saturation core, but the loop compensation has to be designed for the inductance that remains.
Energy storage at the saturation current is around 231 uJ, the number that connects the inductance and the current rating into a single transient figure.
The second saturation column, 86.5 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.
The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.
The HC7 family spans 0.22 uH to 4.81 uH; this row sits at position 1 of 7.
The next value up in the same family, HC7-R47-R, gives 0.53 uH at 23.4 A and DCR 1.6 mOhm: the extra inductance costs about 0 A of rated current.
Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 0.67 mOhm becomes roughly 1.03 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.
Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.
Does the inductance drift with age?
The binder is non-organic and the core is not gapped with adhesive, so thermal aging of the magnetic path is not a mechanism here. The value is stable across thermal cycles.
How do I estimate the inductance at my operating current?
Read it off the inductance-versus-DC-bias curve in the data sheet at the actual bias. The curve, not the OCL value, is what sets the ripple at load.
Which saturation column should I design to?
The one that matches the inductance droop your loop can tolerate. The 30 % column gives a higher usable peak current; the tighter column keeps more inductance at the cost of headroom.