| Parameter | Value |
|---|---|
| Orderable part number | HC8LP-3R5-R |
| OCL (open circuit inductance) | 3.56 uH ±20% |
| Irms (DC, 40 °C rise) | 6.9 A |
| Isat (15% rolloff) | 6.4 A |
| Isat2 (30% rolloff) | 11.4 A |
| DCR typical @ +20 °C | 24.5 mOhm |
| Volt-time rating (V-us) | 5.6 |
| Package | 10.9 x 10.4 mm |
| Height | 3.5 mm |
| Mounting | Surface mount |
| Operating temperature | -40 °C to +155 °C (ambient plus self-heating) |
| Qualification | Commercial grade |
| RoHS | Compliant, -R suffix |
| Data sheet | Eaton Technical Data 4126 |

Drawing reproduced from Eaton Technical Data 4126: outline with
rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
the drawing itself.
This is a surface-mount inductor on a distributed air gap: the powder core spreads the gap through the whole volume, which is why the part tolerates large DC bias without a cliff in the inductance curve, and why it is used on multiphase rails where the inductors share current.
At the rated 6.9 A the winding dissipates about 1.17 W in copper alone, using the typical DCR of 24.5 mOhm. That figure is the floor of the loss budget: it assumes the current is pure DC, and any ripple adds to it.
Saturation is quoted as 15% rolloff. At that point the inductance has fallen to the stated fraction of its nominal value – the part is not damaged there, it simply stops behaving like the inductance on the label. Design the peak current to stay inside that boundary with margin for tolerance.
Energy storage at the saturation current is around 72.9 uJ, the number that connects the inductance and the current rating into a single transient figure.
The second saturation column, 11.4 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.
The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.
The HC8LP family spans 0.17 uH to 47.9 uH; this row sits at position 7 of 16.
Compared with its neighbours in the table, HC8LP-4R5-R trades 1.8 A of rated current for the next inductance step, which is the usual compromise in this family.
Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 24.5 mOhm becomes roughly 37.5 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.
Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.
Which saturation column should I design to?
The one that matches the inductance droop your loop can tolerate. The 30 % column gives a higher usable peak current; the tighter column keeps more inductance at the cost of headroom.
Does the inductance drift with age?
The binder is non-organic and the core is not gapped with adhesive, so thermal aging of the magnetic path is not a mechanism here. The value is stable across thermal cycles.
Is the part shielded?
The winding is enclosed by the powder core, so the external field is small. It is not a closed ferrite shield, but the fringing field is low enough for dense board layouts.