| Parameter | Value |
|---|---|
| Orderable part number | HC9-1R5-R |
| OCL (open circuit inductance) | 1.70 uH ±15% |
| Irms (DC, 40 °C rise) | 21 A |
| Isat (20% rolloff) | 22 A |
| Isat2 (30% rolloff) | 32 A |
| DCR typical @ +20 °C | 2.27 mOhm |
| Volt-time rating (V-us) | 8.46 |
| Package | 13.1 x 14.1 mm |
| Height | 7.5 mm |
| Mounting | Surface mount |
| Operating temperature | -40 °C to +155 °C (ambient plus self-heating) |
| Qualification | Commercial grade |
| RoHS | Compliant, -R suffix |
| Data sheet | Eaton Technical Data DS4312 |

Drawing reproduced from Eaton Technical Data DS4312: outline with
rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
the drawing itself.
Powder iron is the material choice that gives this family its soft saturation curve and its stable inductance over temperature. There is no thermal aging of the binder, so the inductance you measure on day one is the inductance you have after a thousand thermal cycles.
The DCR figure of 2.27 mOhm is what sets the efficiency: at 21 A the winding drops about 0.048 mV and dissipates 1 W. On a low-voltage rail that drop is a measurable fraction of the output, so the DCR column deserves as much attention as the inductance.
The Isat column is 20% rolloff. Note what it does and does not mean: it is a defined rolloff point, not a destruction limit. Above it the inductance continues to fall, which is why the transient peak current should be checked against the curve, not just against the number.
Energy storage at the saturation current is around 411 uJ, the number that connects the inductance and the current rating into a single transient figure.
The second saturation column, 32 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.
The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.
Within the HC9 family this is value 4 of 12, in a range that runs from 0.218 uH to 49.2 uH.
One step down the table, HC9-1R0-R, sits at 1.04 uH with 23.7 A and 1.87 mOhm – the lower inductance buys about 6.5 A of extra current in the same body.
Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 2.27 mOhm becomes roughly 3.47 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.
Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.
How do I estimate the inductance at my operating current?
Read it off the inductance-versus-DC-bias curve in the data sheet at the actual bias. The curve, not the OCL value, is what sets the ripple at load.
Why is the DCR higher than a ferrite part of the same size?
Iron powder has lower permeability, so more turns are needed for the same inductance, and more turns mean more copper. The compensation is the much higher saturation flux density.
Is the part shielded?
The winding is enclosed by the powder core, so the external field is small. It is not a closed ferrite shield, but the fringing field is low enough for dense board layouts.
Shenzhen Gaorunxin Technology Co., Ltd
Shenzhen Gaorunxin Technology Co., Ltd